Why do the pigments are in liquid form?
In BCP, we have been manufacturing since 1962 resins and additives, being almost 50 years we have been producing monolayers and colored cementitious products inside and out.
The pigment does not fade, do not fade and the quality of our product line aims to offer is an initial source of pigment solid state. (Dust) within the range of solid pigments, we work with the best quality. (Thousands of works of monolayer services throughout our history behind us)
For us it is very easy to mix the necessary proportion of dust in the cube have micro, but it is not properly correct for several reasons:
The pigment dilution takes quality (can appear flat when passing tear caused by a grain of undissolved pigment and causes a wake bay shooting mode to decomposition) Understand that dissolve easily but 80% of the pigment , and with effort 90 to 95%, only 1% that does not dissolve and ruin the application (10 / 12 lines per m2).
 |
If the pigment was in liquid water as those sold in the market by dissolving pigmentosa brilliantly, but using liquid pigment, remember that it is not the same quality, and also adversely affects the mix microcemento, and the pigment-based liquid is water and if the mixture needs of 10 kg have micro (MC) or micro-concrete (MH), 4 liters of resin, pigment if it takes 1 liter of water, only enter the 3 liters of resin mixture, so that the hardness is affected by 20%. Besides being pigments that resist radiation or alkalinity.
BCP, the pigment used in the solid state to liquid transformed in this way, the same type of high-quality pigment for mortar and monolayers, using a chemical process at the atomic level desfracmentamos pigments and then additive alloys, we transform the pigment in a liquid state, where this process is added to the mix additive value of hardness and plasticity necessary. |
The mixture is provided a container of pigment by a container of any product in our dust, so each product has a certain type of Kg.
If on the other hand you want to add pigment tilts grams, is quite simple:
1 -. although the pigment and the pigment weight divided by the MC or MH Kg has raw (coming grams per kilogram of pigment MC or MH)
2 -. select few kg of MC or MH, you put utilizar.y grams per kg previously calculated for each kg of MC or MH desired.
Never have a different tone with this practice, but if you want more complicated formats can ask young as 5 or 10 pounds and make the mixture 100% 100% pigment dust.
Free consultation with our technician.
Do not be fooled by other manufacturers cases, just because they do not have the means to provide the best quality with the best system compatible with your application.
Because microconcrete recommend microcemento and bicomponent? (Powder + liquid resin)
It is very simple, BCP, may include solid state liquid resin in powder form in the product mix, but do not because it is not advisable for several reasons more than evident.
1 -. Higher quality resins, cost more to dissolve, and have ever heard to use a tile adhesive for porcelain or facades of quality in the "Technical Guide ceramic tile installation" is recommended once beaten the product, is expected to be well dissolved resins, and once after 5 minutes, whisk again for resins dissolved and re-mix accordingly.
2 -. As in the case of cement glue, this is not going well pigmented and is not seen, because the tile is going up, more significance is not appreciated as mentioned above, but in the case of MC or MH, which is a finishing product, remember that it's interesting because we need the two-component resin mixture is properly made. (When the liquid resin and resin dissolved supplied). We must not leave the responsibility for the worker who may or may not have enough left to stand, you can more or less cold and can help more or less to the mix (a colder later in the resin dissolved, as a typical chocolate bar)
3 -. Furthermore, since the material is pigmented, and if served whole powder, when mixed with normal water thinking there's a final savings, false details, because if one goes all the dust, the more expensive by increasing resin, mineral salts and lime, will be reflected in the application with white or reduced color barbaric way unwanted irregular shape.
 |
|
Therefore, we do recommend that if manufacturers or their official distributors with experience in the industry and especially with more experience in product range (mortars, cements, adhesive, waterproofing, monolayers, paintings, acrylic coatings, maplexine, granulite, stucco Venetian ...) because all previously known makes all the reactions of the materials sold, and can always offer the best quality at more than evident good price.
It is best to use liquid resin prepared for the applicator to give the guarantee and the certainty of a good application, both in labor and material in optimum quality.
What to do if I have wet temperatures, extremely dry or drafty for the application.
Consult with tel. Customer Service 969 100 100, because it will go through the Disc.Technical and they will advise you free product to use for each case and even fit a specific product for each time because we are manufacturers as well as product developers even for third party brands.
It is important if the spell of damp media that is waterproof and will help us not to transmit moisture.
Yet if other than the support base is moist and is corrected with the spell of media, if the environment is too, we know that can not be varnished with lacquer solvent, except that we provide a suitable primer for it or chemically modify the product you for it.
Of all must be known that the solvent (brand whatever) to contact with the water whitens and softens with moisture.

If we draft, we can dehydrate microcemento application as if it were our skin in the cold of winter, so we would create microcracks in the firm, but in the case of applying the water-component coating it would be hard top and soft on the inside, as if a door painted with a brush is treated as conventional paint with fingernail mark and brand, that is too superficial layer and dried, but delay the process harden , so the application would probably dry marked by the heels or daily.
If the above process was a solvent coating, hardening lead to higher output of non-catalyst and the effect of this would have thrown more so due reblandecería lacquer and solvent vapor also would not leave because the rhythm and this reblandecería the entire system even have micro layers thick.
For use in extreme cases contact BCP, our experience and our product portfolio we can give will be the right solution. We recall that as product development company, we can manufacture a custom product for any given situation.